Cause:

1. The rough and bad pre-treatment of workpiece.

2. The curing time is too long or the temperature of curing oven is too high.

3. There are volatile gases in the furnace.

4. The proportion of recycled powder is too large.

5. Two different types of powder mix.

6. Poor quality of powder.

Solution:

1. Select the appropriate pretreatment process.

2. Adjust the appropriate curing conditions.

3. Clean the oven.

4. After the recycled powder is filtered, it should be mixed with fresh powder, preferably less than 30%.

5. Thoroughly clean the dusting system before powder change.

6. Replace the good quality powder.


Find more info, pls contact

Sale Manager: Jenny Wu

Phone/Whatsapp/Wechat: 0086 186 3304 5156


Contact us

Customer Satisfaction Guarantee for Powder Coating Equipment Manufacturers: The Key to Quality and Service

Streamlining Production Efficiency: 4 Advantages of an Automatic Conveyor System

Discover the future of coating technology: We invite you to the SprayTec Germany!

Exploring the difference between matte coating formed by powder coating and ordinary coating

Powder Recycling Technology in Powder Coating Equipment: Key Challenges and Innovative Solutions